How to Identify a Weak Cell in a Lithium Battery Pack

A lithium battery pack can contain multiple cells or parallel cell groups connected together to provide the required voltage and capacity. When one cell or cell group develops a problem, the entire battery pack may show abnormal behavior.

A weak cell does not always fail completely. It may still show a normal voltage when the battery is resting but behave differently from the other cells during charging or discharging.

Identifying a weak cell requires more than checking the total battery voltage. Cell-group voltage, voltage difference, internal resistance, capacity, temperature, and behavior under load can all provide useful information.

This guide explains how to identify a weak cell or cell group in a lithium battery pack and what factors should be considered during battery diagnosis.

lithium battery pack.

1. What Is a Weak Cell?

A weak cell is a cell that does not perform within the expected range of the other cells in the same battery pack.

The term can refer to different conditions, including:

  • Lower capacity
  • Higher internal resistance
  • Abnormal voltage behavior
  • Faster voltage drop under load
  • Faster voltage rise during charging
  • Higher self-discharge
  • Abnormal temperature increase
  • Increased voltage difference within a series-connected pack

In a battery pack containing cells connected in series, the cells share the same charging and discharging current. If one cell reaches its voltage limit earlier than the others, the BMS may stop charging or discharging to protect the pack.

Therefore, one weak cell can affect the usable performance of the entire battery pack.

2. Why Can One Weak Cell Affect the Whole Battery Pack?

Consider a battery pack made from several cell groups connected in series.

The total voltage is the sum of the voltage of each series group.

例えば、こうだ:

Pack voltage = Cell Group 1 + Cell Group 2 + Cell Group 3 + Cell Group 4 + …

If one group has lower voltage than the others, the total pack voltage may still appear normal under some conditions.

However, during discharge, the weak group may reach the lower voltage limit earlier.

During charging, the same group may also behave differently from the other groups.

This can cause the BMS to trigger undervoltage or overvoltage protection even when the total pack voltage does not initially appear abnormal.

3. Start With Cell-Group Voltage

Cell-group voltage is one of the basic parameters used when checking battery condition.

For a battery pack with cells connected in series, measure the voltage of each series group according to the battery manufacturer’s testing procedure.

Compare the readings under the same operating condition.

For example, if several groups show similar voltages while one group has a noticeable deviation, that group requires further inspection.

However, voltage difference alone does not prove that a cell is defective.

Voltage can change with:

  • 充電状態
  • 温度
  • Charging or discharging current
  • Resting time
  • 細胞化学
  • Cell age

For this reason, voltage should be evaluated together with other test results.

4. Check Cell Voltage After Resting

Battery voltage changes during charging and discharging.

Immediately after charging, the voltage of individual cells may not represent their equilibrium condition. The same applies immediately after a high-current discharge.

A resting-voltage check can provide additional information.

A typical diagnostic process may involve:

  1. Fully charge the battery according to the manufacturer’s specifications.
  2. Allow the battery to rest for the specified period.
  3. Measure each cell group.
  4. Record the voltage of each group.
  5. Compare the readings.

The required charging voltage, resting time, and acceptable voltage range depend on the cell chemistry and battery design.

The purpose of the test is to compare cells under the same conditions.

5. Monitor Voltage Difference During Discharge

A weak cell may become easier to identify when the battery is under load.

Suppose several cell groups start at similar voltages.

During discharge:

  • Normal groups may maintain relatively similar voltage behavior.
  • A weak group may show a larger voltage drop.
  • The weak group may reach the BMS undervoltage threshold earlier.

This is known as voltage sag under load.

Voltage sag is affected by internal resistance and current.

関係を簡略化すると、次のようになります:

Voltage drop ≈ Current × Internal Resistance

If the internal resistance of one cell group is higher, its voltage may drop more when the discharge current increases.

A controlled load test can therefore provide information that is not available from a simple open-circuit voltage measurement.

6. Measure Internal Resistance

Internal resistance is another parameter used to evaluate cell condition.

As a cell ages or develops an internal problem, its internal resistance may increase.

When current flows through the cell, the voltage response is affected by its internal resistance.

A cell with higher resistance may show:

  • Larger voltage drop during discharge
  • Greater voltage rise during charging
  • More heat generation under load
  • Reduced usable energy under certain operating conditions

Internal resistance should be measured using an appropriate battery tester and under consistent conditions.

Different testing instruments can use different measurement methods, so readings from different instruments should not always be compared directly.

The resistance value should also be considered together with cell model, temperature, SOC, and test method.

7. Compare Capacity

Capacity testing can help determine whether a cell or cell group can deliver the expected amount of energy.

For example, a battery pack may show acceptable voltage during a short test but provide less runtime than expected.

A controlled discharge test can measure the available capacity.

The general relationship is:

Capacity (Ah) = Current (A) × Discharge Time (h)

For example, if a battery delivers 10 A for 2 hours under the specified test conditions:

10 A × 2 h = 20 Ah

For a battery pack containing series-connected groups, the capacity of the series string is limited by the cell group with the available capacity required by the pack design.

Capacity testing should be performed using the manufacturer’s specified charge, discharge current, voltage limits, and temperature conditions.

8. Check Self-Discharge

A cell can also show abnormal behavior when the battery is not being used.

If one cell group loses voltage faster than the others during storage, it may indicate:

  • Increased self-discharge
  • Cell degradation
  • Leakage current
  • BMS-related current imbalance
  • A connection or measurement issue

A controlled self-discharge test requires the battery to be monitored over an appropriate period.

Before concluding that a cell is defective, verify that the BMS and measurement system are not causing the observed voltage difference.

9. Check Temperature

Temperature can provide another indication of abnormal cell behavior.

During charging or discharging, compare the temperature of the cell groups under the same operating conditions.

A cell group that becomes noticeably warmer than the others may require further inspection.

Possible causes include:

  • 内部抵抗の増加
  • 過電流
  • Poor electrical connection
  • Cell degradation
  • Localized electrical resistance
  • External thermal conditions

Temperature alone does not identify the exact cause.

Thermal measurements should therefore be combined with voltage, resistance, current, and capacity data.

10. Use BMS Data to Identify Abnormal Cell Groups

A smart BMS may provide individual cell or cell-group information.

Depending on the BMS, available data may include:

  • Cell-group voltage
  • パック電圧
  • 現在
  • 温度
  • SOC
  • 保護状況
  • Cell voltage difference
  • 充電状況
  • 放電状態

This information can help identify a cell group that behaves differently from the others.

For example, if one cell group repeatedly reaches the undervoltage protection threshold before the other groups, it may require further testing.

However, BMS data should be verified against appropriate electrical measurements when diagnosing a suspected cell fault.

A displayed value can also be affected by voltage-sensing wiring, calibration, communication errors, or BMS configuration.

11. Check the Battery Under Different Conditions

A weak cell may not be obvious under one operating condition.

For this reason, testing can include several conditions:

Resting Condition

Measure cell-group voltage after the battery has rested.

Charging Condition

Monitor how each group responds during charging.

Discharging Condition

Monitor voltage behavior while the battery supplies a controlled load.

High-Current Condition

If permitted by the battery design, observe the voltage response at an appropriate current level.

Recovery Condition

After the load is removed, monitor how the cell-group voltage recovers.

Comparing these conditions can help distinguish between normal voltage variation and abnormal cell behavior.

12. Look for Repeated Voltage Imbalance

A single voltage difference does not necessarily mean that a cell is weak.

For example, voltage differences can occur because the cells are at different SOC levels.

A stronger indication is a voltage imbalance that repeatedly appears under similar operating conditions.

A diagnostic process can therefore record cell-group voltage over multiple cycles.

If the same group repeatedly:

  • Drops to a lower voltage during discharge
  • Reaches a higher voltage during charging
  • Shows a larger voltage change
  • Triggers BMS protection
  • Shows increased resistance

that group may require additional inspection.

13. Check the BMS Before Replacing a Cell

Not every abnormal cell voltage is caused by a damaged cell.

Before replacing a cell or cell group, check the BMS and sensing circuit.

Possible causes of an abnormal reading include:

  • Loose sensing wire
  • Damaged sensing wire
  • Poor connector contact
  • Incorrect BMS configuration
  • Measurement error
  • BMS calibration issue
  • Communication error

If the BMS reports one cell group at an abnormal voltage, compare the BMS reading with a suitable direct measurement performed according to the battery service procedure.

This can help determine whether the problem is located in the cell or in the measurement system.

14. Common Signs of a Weak Cell

The following symptoms may indicate that a cell or cell group requires inspection:

  • Large voltage difference between cell groups
  • One group reaches undervoltage protection earlier
  • One group reaches overvoltage protection during charging
  • Abnormal voltage drop under load
  • 内部抵抗の増加
  • 使用可能容量の減少
  • Faster self-discharge
  • Abnormal temperature rise
  • Reduced runtime
  • Repeated BMS protection events

These signs should be evaluated together rather than used individually as proof of cell failure.

15. Can a Weak Cell Be Replaced?

Whether a weak cell can be replaced depends on the battery construction, cell type, pack design, BMS configuration, and service requirements.

For a battery pack containing multiple series-connected cells, replacing one cell with a new cell can create differences in:

  • 定員
  • 内部抵抗
  • SOC
  • Aging state
  • Voltage characteristics

If cell replacement is required, the replacement cell should meet the specifications of the original pack design.

The battery may also require balancing and testing after service.

For sealed battery packs or packs used in safety-critical equipment, service should be performed by qualified personnel according to the applicable procedures.

16. When Should a Battery Pack Be Removed From Service?

Stop using the battery and arrange appropriate inspection if it shows:

  • むくみ
  • Leakage
  • Physical damage
  • Burn marks
  • 異常な発熱
  • Unusual odor
  • Repeated protection events
  • Severe cell voltage imbalance
  • Suspected internal short circuit

Do not continue charging or discharging a battery that shows signs of physical damage or abnormal heating.

17. How to Test a Lithium Battery Pack for a Weak Cell

A practical diagnostic sequence can be organized as follows:

Step 1: Record the battery model, chemistry, rated voltage, and capacity.

Step 2: Inspect the battery pack and wiring.

Step 3: Check the BMS status and available cell-group data.

Step 4: Measure cell-group voltage under a consistent resting condition.

Step 5: Check the voltage difference between groups.

Step 6: Measure internal resistance using an appropriate tester.

Step 7: Perform a controlled charge and discharge test when required.

Step 8: Monitor voltage behavior under load.

Step 9: Check temperature during operation.

Step 10: Compare the results with the cell and battery manufacturer’s specifications.

This process provides multiple data points instead of relying on a single voltage measurement.

18. How to Reduce Cell Imbalance During Battery Design

Cell consistency should be considered during battery pack design.

重要な要素としては、以下のものが挙げられます:

  • 細胞の選択
  • セルの照合
  • 直列接続と並列接続
  • BMSの設定
  • Cell balancing method
  • 現在の要件
  • 熱管理
  • Protection settings
  • Manufacturing process
  • Quality inspection

The battery pack should be designed around the electrical and environmental requirements of the target application.

For custom lithium battery packs, the cell type, pack configuration, BMS functions, operating current, temperature range, and testing requirements can be defined during the design stage.

結論

Identifying a weak cell in a lithium battery pack requires more than checking the total pack voltage.

Cell-group voltage, voltage difference, internal resistance, capacity, self-discharge, temperature, and load behavior can provide information about cell condition.

A suspected weak cell should be evaluated under consistent test conditions, and BMS data should be checked together with electrical measurements.

If a battery shows physical damage, abnormal heating, severe voltage imbalance, or repeated protection events, it should be removed from service until the cause has been evaluated.

For custom battery packs, cell selection, BMS configuration, balancing, thermal design, and testing can be considered together during battery development. This allows the battery design to match the electrical and operating requirements of the intended application.

Learn how to identify a weak cell in a lithium battery pack. Check cell voltage, voltage difference, internal resistance, capacity, temperature, and BMS data.
2026-11-27
+
Learn how cold weather affects lithium batteries and how to maintain them safely. Discover tips for charging, storage, discharge, BMS protection, and low-temperature battery design.
2026-11-27
+
Learn how to prevent lithium battery capacity loss during storage. Discover proper SOC, temperature, storage conditions, and maintenance practices to extend battery life.
2026-11-26
+
Learn about lithium battery pack design for compact electric construction equipment, including LiFePO4 cells, voltage, current, BMS, charging and vibration protection.
2026-11-25
+