A lithium battery pack can contain multiple cells or parallel cell groups connected together to provide the required voltage and capacity. When one cell or cell group develops a problem, the entire battery pack may show abnormal behavior.
A weak cell does not always fail completely. It may still show a normal voltage when the battery is resting but behave differently from the other cells during charging or discharging.
Identifying a weak cell requires more than checking the total battery voltage. Cell-group voltage, voltage difference, internal resistance, capacity, temperature, and behavior under load can all provide useful information.
This guide explains how to identify a weak cell or cell group in a lithium battery pack and what factors should be considered during battery diagnosis.

1. What Is a Weak Cell?
A weak cell is a cell that does not perform within the expected range of the other cells in the same battery pack.
The term can refer to different conditions, including:
- Lower capacity
- Higher internal resistance
- Abnormal voltage behavior
- Faster voltage drop under load
- Faster voltage rise during charging
- Higher self-discharge
- Abnormal temperature increase
- Increased voltage difference within a series-connected pack
In a battery pack containing cells connected in series, the cells share the same charging and discharging current. If one cell reaches its voltage limit earlier than the others, the BMS may stop charging or discharging to protect the pack.
Therefore, one weak cell can affect the usable performance of the entire battery pack.
2. Why Can One Weak Cell Affect the Whole Battery Pack?
Consider a battery pack made from several cell groups connected in series.
The total voltage is the sum of the voltage of each series group.
Par exemple :
Pack voltage = Cell Group 1 + Cell Group 2 + Cell Group 3 + Cell Group 4 + …
If one group has lower voltage than the others, the total pack voltage may still appear normal under some conditions.
However, during discharge, the weak group may reach the lower voltage limit earlier.
During charging, the same group may also behave differently from the other groups.
This can cause the BMS to trigger undervoltage or overvoltage protection even when the total pack voltage does not initially appear abnormal.
3. Start With Cell-Group Voltage
Cell-group voltage is one of the basic parameters used when checking battery condition.
For a battery pack with cells connected in series, measure the voltage of each series group according to the battery manufacturer’s testing procedure.
Compare the readings under the same operating condition.
For example, if several groups show similar voltages while one group has a noticeable deviation, that group requires further inspection.
However, voltage difference alone does not prove that a cell is defective.
Voltage can change with:
- State of charge
- Température
- Charging or discharging current
- Resting time
- Chimie cellulaire
- Cell age
For this reason, voltage should be evaluated together with other test results.
4. Check Cell Voltage After Resting
Battery voltage changes during charging and discharging.
Immediately after charging, the voltage of individual cells may not represent their equilibrium condition. The same applies immediately after a high-current discharge.
A resting-voltage check can provide additional information.
A typical diagnostic process may involve:
- Fully charge the battery according to the manufacturer’s specifications.
- Allow the battery to rest for the specified period.
- Measure each cell group.
- Record the voltage of each group.
- Compare the readings.
The required charging voltage, resting time, and acceptable voltage range depend on the cell chemistry and battery design.
The purpose of the test is to compare cells under the same conditions.
5. Monitor Voltage Difference During Discharge
A weak cell may become easier to identify when the battery is under load.
Suppose several cell groups start at similar voltages.
During discharge:
- Normal groups may maintain relatively similar voltage behavior.
- A weak group may show a larger voltage drop.
- The weak group may reach the BMS undervoltage threshold earlier.
This is known as voltage sag under load.
Voltage sag is affected by internal resistance and current.
A simplified relationship is:
Voltage drop ≈ Current × Internal Resistance
If the internal resistance of one cell group is higher, its voltage may drop more when the discharge current increases.
A controlled load test can therefore provide information that is not available from a simple open-circuit voltage measurement.
6. Measure Internal Resistance
Internal resistance is another parameter used to evaluate cell condition.
As a cell ages or develops an internal problem, its internal resistance may increase.
When current flows through the cell, the voltage response is affected by its internal resistance.
A cell with higher resistance may show:
- Larger voltage drop during discharge
- Greater voltage rise during charging
- More heat generation under load
- Reduced usable energy under certain operating conditions
Internal resistance should be measured using an appropriate battery tester and under consistent conditions.
Different testing instruments can use different measurement methods, so readings from different instruments should not always be compared directly.
The resistance value should also be considered together with cell model, temperature, SOC, and test method.
7. Compare Capacity
Capacity testing can help determine whether a cell or cell group can deliver the expected amount of energy.
For example, a battery pack may show acceptable voltage during a short test but provide less runtime than expected.
A controlled discharge test can measure the available capacity.
The general relationship is:
Capacity (Ah) = Current (A) × Discharge Time (h)
For example, if a battery delivers 10 A for 2 hours under the specified test conditions:
10 A × 2 h = 20 Ah
For a battery pack containing series-connected groups, the capacity of the series string is limited by the cell group with the available capacity required by the pack design.
Capacity testing should be performed using the manufacturer’s specified charge, discharge current, voltage limits, and temperature conditions.
8. Check Self-Discharge
A cell can also show abnormal behavior when the battery is not being used.
If one cell group loses voltage faster than the others during storage, it may indicate:
- Increased self-discharge
- Cell degradation
- Leakage current
- BMS-related current imbalance
- A connection or measurement issue
A controlled self-discharge test requires the battery to be monitored over an appropriate period.
Before concluding that a cell is defective, verify that the BMS and measurement system are not causing the observed voltage difference.
9. Check Temperature
Temperature can provide another indication of abnormal cell behavior.
During charging or discharging, compare the temperature of the cell groups under the same operating conditions.
A cell group that becomes noticeably warmer than the others may require further inspection.
Possible causes include:
- Augmentation de la résistance interne
- Courant excessif
- Poor electrical connection
- Cell degradation
- Localized electrical resistance
- External thermal conditions
Temperature alone does not identify the exact cause.
Thermal measurements should therefore be combined with voltage, resistance, current, and capacity data.
10. Use BMS Data to Identify Abnormal Cell Groups
A smart BMS may provide individual cell or cell-group information.
Depending on the BMS, available data may include:
- Cell-group voltage
- Tension du bloc-batterie
- Actuel
- Température
- SOC
- Statut de protection
- Cell voltage difference
- État de charge
- Discharging status
This information can help identify a cell group that behaves differently from the others.
For example, if one cell group repeatedly reaches the undervoltage protection threshold before the other groups, it may require further testing.
However, BMS data should be verified against appropriate electrical measurements when diagnosing a suspected cell fault.
A displayed value can also be affected by voltage-sensing wiring, calibration, communication errors, or BMS configuration.
11. Check the Battery Under Different Conditions
A weak cell may not be obvious under one operating condition.
For this reason, testing can include several conditions:
Resting Condition
Measure cell-group voltage after the battery has rested.
Charging Condition
Monitor how each group responds during charging.
Discharging Condition
Monitor voltage behavior while the battery supplies a controlled load.
High-Current Condition
If permitted by the battery design, observe the voltage response at an appropriate current level.
Recovery Condition
After the load is removed, monitor how the cell-group voltage recovers.
Comparing these conditions can help distinguish between normal voltage variation and abnormal cell behavior.
12. Look for Repeated Voltage Imbalance
A single voltage difference does not necessarily mean that a cell is weak.
For example, voltage differences can occur because the cells are at different SOC levels.
A stronger indication is a voltage imbalance that repeatedly appears under similar operating conditions.
A diagnostic process can therefore record cell-group voltage over multiple cycles.
If the same group repeatedly:
- Drops to a lower voltage during discharge
- Reaches a higher voltage during charging
- Shows a larger voltage change
- Triggers BMS protection
- Shows increased resistance
that group may require additional inspection.
13. Check the BMS Before Replacing a Cell
Not every abnormal cell voltage is caused by a damaged cell.
Before replacing a cell or cell group, check the BMS and sensing circuit.
Possible causes of an abnormal reading include:
- Loose sensing wire
- Damaged sensing wire
- Poor connector contact
- Incorrect BMS configuration
- Measurement error
- BMS calibration issue
- Communication error
If the BMS reports one cell group at an abnormal voltage, compare the BMS reading with a suitable direct measurement performed according to the battery service procedure.
This can help determine whether the problem is located in the cell or in the measurement system.
14. Common Signs of a Weak Cell
The following symptoms may indicate that a cell or cell group requires inspection:
- Large voltage difference between cell groups
- One group reaches undervoltage protection earlier
- One group reaches overvoltage protection during charging
- Abnormal voltage drop under load
- Augmentation de la résistance interne
- Réduction de la capacité utilisable
- Faster self-discharge
- Abnormal temperature rise
- Reduced runtime
- Repeated BMS protection events
These signs should be evaluated together rather than used individually as proof of cell failure.
15. Can a Weak Cell Be Replaced?
Whether a weak cell can be replaced depends on the battery construction, cell type, pack design, BMS configuration, and service requirements.
For a battery pack containing multiple series-connected cells, replacing one cell with a new cell can create differences in:
- Capacité
- Résistance interne
- SOC
- Aging state
- Voltage characteristics
If cell replacement is required, the replacement cell should meet the specifications of the original pack design.
The battery may also require balancing and testing after service.
For sealed battery packs or packs used in safety-critical equipment, service should be performed by qualified personnel according to the applicable procedures.
16. When Should a Battery Pack Be Removed From Service?
Stop using the battery and arrange appropriate inspection if it shows:
- Gonflement
- Leakage
- Physical damage
- Burn marks
- Abnormal heating
- Unusual odor
- Repeated protection events
- Severe cell voltage imbalance
- Suspected internal short circuit
Do not continue charging or discharging a battery that shows signs of physical damage or abnormal heating.
17. How to Test a Lithium Battery Pack for a Weak Cell
A practical diagnostic sequence can be organized as follows:
Step 1: Record the battery model, chemistry, rated voltage, and capacity.
Step 2: Inspect the battery pack and wiring.
Step 3: Check the BMS status and available cell-group data.
Step 4: Measure cell-group voltage under a consistent resting condition.
Step 5: Check the voltage difference between groups.
Step 6: Measure internal resistance using an appropriate tester.
Step 7: Perform a controlled charge and discharge test when required.
Step 8: Monitor voltage behavior under load.
Step 9: Check temperature during operation.
Step 10: Compare the results with the cell and battery manufacturer’s specifications.
This process provides multiple data points instead of relying on a single voltage measurement.
18. How to Reduce Cell Imbalance During Battery Design
Cell consistency should be considered during battery pack design.
Parmi les facteurs importants, on peut citer :
- Sélection des cellules
- Correspondance des cellules
- Series and parallel configuration
- Configuration du BMS
- Cell balancing method
- Exigences actuelles
- Gestion thermique
- Protection settings
- Manufacturing process
- Quality inspection
The battery pack should be designed around the electrical and environmental requirements of the target application.
For custom lithium battery packs, the cell type, pack configuration, BMS functions, operating current, temperature range, and testing requirements can be defined during the design stage.
Conclusion
Identifying a weak cell in a lithium battery pack requires more than checking the total pack voltage.
Cell-group voltage, voltage difference, internal resistance, capacity, self-discharge, temperature, and load behavior can provide information about cell condition.
A suspected weak cell should be evaluated under consistent test conditions, and BMS data should be checked together with electrical measurements.
If a battery shows physical damage, abnormal heating, severe voltage imbalance, or repeated protection events, it should be removed from service until the cause has been evaluated.
For custom battery packs, cell selection, BMS configuration, balancing, thermal design, and testing can be considered together during battery development. This allows the battery design to match the electrical and operating requirements of the intended application.